Characterisation and Flotation Studies on Iron Ore Slimes
#0183;#32;From the mineral characterization studies, it was observed that hematite, goethite and martite were iron bearing phases while kaolinite and quartz were its major gangue. The iron ore slimes assayed % Fe with % SiO2 and % Al2O3. The sample deslimed prior to flotation using hydrocylone to remove the ultrafine particles.